![](/img/cover-not-exists.png)
Surface recrystallization of single crystal nickel-based superalloy
ZHANG, Bing, CAO, Xue-gang, LIU, De-lin, LIU, Xin-lingVolume:
23
Language:
english
Journal:
Transactions of Nonferrous Metals Society of China
DOI:
10.1016/S1003-6326(13)62595-9
Date:
May, 2013
File:
PDF, 5.05 MB
english, 2013