![](/img/cover-not-exists.png)
Modulated differential scanning calorimetry in the glass transition region. Part III. Evaluation of polystyrene and poly(ethylene tetrephthalate)
Andreas Boller, Iwao Okazaki, Bernhard WunderlichVolume:
284
Year:
1996
Language:
english
Pages:
19
DOI:
10.1016/0040-6031(96)02865-1
File:
PDF, 798 KB