![](/img/cover-not-exists.png)
TLP bonding of cast IN718 nickel based superalloy: Process–microstructure–strength characteristics
Pouranvari, M., Ekrami, A., Kokabi, A.H.Volume:
568
Language:
english
Journal:
Materials Science and Engineering: A
DOI:
10.1016/j.msea.2013.01.029
Date:
April, 2013
File:
PDF, 1.41 MB
english, 2013