![](/img/cover-not-exists.png)
Stress rupture properties of GH4169 superalloy
Lu, Xudong, Du, Jinhui, Deng, Qun, Zhuang, JingyunVolume:
3
Language:
english
Journal:
Journal of Materials Research and Technology
DOI:
10.1016/j.jmrt.2014.03.003
Date:
April, 2014
File:
PDF, 3.33 MB
english, 2014