Influence of residual compressive stress on nanoindentation response of ion-exchanged aluminosilicate float glass on air and tin sides
Li, Xiaoyu, Jiang, Liangbao, Zhang, Xiaowen, Yan, YueVolume:
385
Language:
english
Journal:
Journal of Non-Crystalline Solids