International Journal of Materials Research (formerly Zeitschrift fuer Metallkunde)
2014 / 04 Vol. 105; Iss. 4
![](/img/cover-not-exists.png)
Hot ductility behavior of Incoloy901 superalloy in the cast and wrought conditions
Shore, Fatemeh Mohammadi, Morakabati, Maryam, Mahdavi, RashidVolume:
105
Language:
english
Journal:
International Journal of Materials Research
DOI:
10.3139/146.111029
Date:
April, 2014
File:
PDF, 2.52 MB
english, 2014