![](/img/cover-not-exists.png)
Heat treatments of the low-expansion superalloy Incoloy 909 for application in ceramic/metal joints and in metal matrix composites
R. Larker, K. Anevik, S. Kristiansson, B. LobergVolume:
13
Year:
1992
Language:
english
Pages:
5
DOI:
10.1016/0261-3069(92)90046-k
File:
PDF, 1.04 MB
english, 1992