Reduced Dwell-Fatigue Resistance in a Ni-Base Superalloy After Short-Term Thermal Exposure
Hörnqvist, Magnus, Viskari, LeifVolume:
45
Language:
english
Journal:
Metallurgical and Materials Transactions A
DOI:
10.1007/s11661-014-2291-4
Date:
June, 2014
File:
PDF, 1021 KB