The effects of ruthenium additions on tensile deformation mechanisms of single crystal superalloys at different temperatures
Wang, X.G., Liu, J.L., Jin, T., Sun, X.F.Volume:
63
Language:
english
Journal:
Materials & Design
DOI:
10.1016/j.matdes.2014.06.009
Date:
November, 2014
File:
PDF, 2.07 MB