![](/img/cover-not-exists.png)
Surface and interface viscoelastic behaviors of thin polymer films investigated by nanoindentation
Zhou, J., Komvopoulos, K.Volume:
100
Year:
2006
Language:
english
Journal:
Journal of Applied Physics
DOI:
10.1063/1.2398797
File:
PDF, 950 KB
english, 2006