Growth of Iron Oxide on Yttria-Stabilized Zirconia by Atomic Layer Deposition
de Ridder, Marco, van de Ven, Patrick C., van Welzenis, Rob G., Brongersma, Hidde H., Helfensteyn, Steve, Creemers, Claude, Van Der Voort, Pascal, Baltes, Michael, Mathieu, Mariska, Vansant, Etienne FVolume:
106
Language:
english
Journal:
The Journal of Physical Chemistry B
DOI:
10.1021/jp0211640
Date:
December, 2002
File:
PDF, 176 KB
english, 2002