![](/img/cover-not-exists.png)
Nucleation-Controlled Growth of Nanoparticles by Atomic Layer Deposition
Lee, Han-Bo-Ram, Mullings, Marja N., Jiang, Xirong, Clemens, Bruce M., Bent, Stacey F.Volume:
24
Language:
english
Journal:
Chemistry of Materials
DOI:
10.1021/cm3014978
Date:
November, 2012
File:
PDF, 2.40 MB
english, 2012