Enhanced stability of cobalt catalysts by atomic layer deposition for aqueous-phase reactions
Lee, Jechan, Jackson, David H. K., Li, Tao, Winans, Randall E., Dumesic, James A., Kuech, Thomas F., Huber, George W.Volume:
7
Year:
2014
Language:
english
Journal:
Energy & Environmental Science
DOI:
10.1039/C4EE00379A