![](/img/cover-not-exists.png)
Enhanced Field Emission Properties from CNT Arrays Synthesized on Inconel Superalloy
Sridhar, S., Ge, L., Tiwary, C. S., Hart, A. C., Ozden, S., Kalaga, K., Lei, S., Sridhar, S. V., Sinha, R. K., Harsh, H., Kordas, K., Ajayan, P. M., Vajtai, R.Volume:
6
Language:
english
Journal:
ACS Applied Materials & Interfaces
DOI:
10.1021/am405026y
Date:
February, 2014
File:
PDF, 420 KB