Effects of silicon content on microstructure and stress corrosion cracking resistance of 7050 aluminum alloy
SHE, Huan, CHU, Wei, SHU, Da, WANG, Jun, SUN, Bao-deVolume:
24
Language:
english
Journal:
Transactions of Nonferrous Metals Society of China
DOI:
10.1016/s1003-6326(14)63349-5
Date:
July, 2014