Corrosive Microenvironments at Lead Solder Surfaces Arising from Galvanic Corrosion with Copper Pipe
Nguyen, Caroline K., Stone, Kendall R., Dudi, Abhijeet, Edwards, Marc A.Volume:
44
Language:
english
Journal:
Environmental Science & Technology
DOI:
10.1021/es1015185
Date:
September, 2010
File:
PDF, 786 KB
english, 2010