Correlation between ultrasonic velocity and solutionising time in Rene 80 superalloy
Aghaie-Khafri, M, Honarvar, F, Zangeneh, SVolume:
27
Language:
english
Journal:
Materials Science and Technology
DOI:
10.1179/026708310x12712410311857
Date:
September, 2011
File:
PDF, 190 KB
english, 2011