Pitting corrosion of triggering initial fractures of palm oil screw press machine shafts
T.M. Loganathan, J. Purbolaksono, J.I. Inayat-Hussain, G. Muthaiyah, N. WahabVolume:
17
Year:
2010
Language:
english
Pages:
8
DOI:
10.1016/j.engfailanal.2010.01.002
File:
PDF, 1.12 MB
english, 2010