![](/img/cover-not-exists.png)
Amorphous vanadium oxide coating on graphene by atomic layer deposition for stable high energy lithium ion anodes
Sun, Xiang, Zhou, Changgong, Xie, Ming, Hu, Tao, Sun, Hongtao, Xin, Guoqing, Wang, Gongkai, George, Steven M., Lian, JieVolume:
50
Language:
english
Journal:
Chemical Communications
DOI:
10.1039/c4cc04580g
Date:
July, 2014
File:
PDF, 1.78 MB
english, 2014