![](/img/cover-not-exists.png)
High-temperature fatigue properties of austenitic superalloys 718, A286 and 304L
Kazuo Kobayashi, Koji Yamaguchi, Masao Hayakawa, Megumi KimuraVolume:
30
Year:
2008
Language:
english
Pages:
7
DOI:
10.1016/j.ijfatigue.2008.01.004
File:
PDF, 1.54 MB
english, 2008