On the interpretation of results from small punch creep tests
Hyde, T H, Stoyanov, M, Sun, W, Hyde, C JVolume:
45
Language:
english
Journal:
The Journal of Strain Analysis for Engineering Design
DOI:
10.1243/03093247jsa592
Date:
April, 2010