![](/img/cover-not-exists.png)
Nanoindentation studies on Cu–Ti–Zr–Ni–Si–Sn bulk metallic glasses
N.K. Mukhopadhyay, A. Belger, P. Paufler, D.H. KimVolume:
449-451
Year:
2007
Language:
english
Pages:
4
DOI:
10.1016/j.msea.2006.02.258
File:
PDF, 384 KB
english, 2007