Effect of heat input on heat affected zone cracking in laser welded ATI Allvac 718Plus superalloy
O.A. Idowu, O.A. Ojo, M.C. ChaturvediVolume:
454-455
Year:
2007
Language:
english
Pages:
9
DOI:
10.1016/j.msea.2006.11.054
File:
PDF, 1.75 MB