![](/img/cover-not-exists.png)
Fractography analysis and fatigue strength of carbon fiber/RTM6 laminates
Maria Odila Hilário Cioffi, Herman Jacobus Cornelis Voorwald, José André Marin Camargo, Mirabel Cerqueira Rezende, Edmundo C. Ortiz, Luigi AmbrosioVolume:
527
Year:
2010
Language:
english
Pages:
6
DOI:
10.1016/j.msea.2010.02.054
File:
PDF, 1.25 MB
english, 2010