Effects of phosphorus segregation on stress corrosion cracking in the heat-affected zone of a dissimilar weld joint between a Ni-base alloy and a low alloy steel
Zhai, Ziqing, Abe, Hiroshi, Miyahara, Yuichi, Watanabe, YutakaVolume:
92
Language:
english
Journal:
Corrosion Science
DOI:
10.1016/j.corsci.2014.10.037
Date:
March, 2015