Influence of alloyed Sc and Zr, and heat treatment on microstructures and stress corrosion cracking of Al–Zn–Mg–Cu alloys
Shi, Yunjia, Pan, Qinglin, Li, Mengjia, Huang, Xing, Li, BoVolume:
621
Language:
english
Journal:
Materials Science and Engineering: A
DOI:
10.1016/j.msea.2014.10.058
Date:
January, 2015