![](/img/cover-not-exists.png)
Atomic layer deposition of functional films for Li-ion microbatteries
Nilsen, Ola, Miikkulainen, Ville, Gandrud, Knut B., Østreng, Erik, Ruud, Amund, Fjellvåg, HelmerVolume:
211
Language:
english
Journal:
physica status solidi (a)
DOI:
10.1002/pssa.201330130
Date:
February, 2014
File:
PDF, 652 KB
english, 2014