Surface Analysis of Cr 2 O 3 -, CoO-, and Al 2 O 3 -Doped Iron-Phosphate Glasses at High Temperature
Yano, Tetsuji, Tateno, Hayato, Kishi, Tetsuo, Shibata, Shuichi, Matsuyama, Kanae, Okita, Takeshi, Miyamoto, Shinya, Kofuji, Hirohide, Myochin, Munetaka, Vance, E.Volume:
97
Language:
english
Journal:
Journal of the American Ceramic Society
DOI:
10.1111/jace.12798
Date:
February, 2014