![](/img/cover-not-exists.png)
A Modified Differential Scanning Calorimetry Method for Determining Water Transport Properties in Biological Cells During the Freezing Process
Han, Xu, Luo, Dawei, Cui, Xiangdong, Heimfeld, Shelly, Gao, DayongVolume:
5
Language:
english
Journal:
Cell Preservation Technology
DOI:
10.1089/cpt.2006.9991
Date:
March, 2007
File:
PDF, 382 KB
english, 2007