Discrete dislocation simulation of nanoindentation: Indentation size effect and the influence of slip band orientation
H.G.M. Kreuzer, R. PippanVolume:
55
Year:
2007
Language:
english
Pages:
7
DOI:
10.1016/j.actamat.2007.01.021
File:
PDF, 759 KB