![](/img/cover-not-exists.png)
Surface analysis of severely corroded coal liquefaction vessel components and model laboratory films
Shalvoy, R. B.Volume:
20
Language:
english
Journal:
Journal of Vacuum Science and Technology
DOI:
10.1116/1.571542
Date:
April, 1982
File:
PDF, 712 KB
english, 1982