In situ quasi-static and dynamic nanoindentation tests on calcified nodules formed by osteoblasts: Implication of glucocorticoids responsible for osteoblast calcification
Miyamoto, Sho, Miyamoto, Yoichi, Shibata, Yo, Yoshimura, Kentaro, Izumida, Eri, Suzuki, Hiroaki, Miyazaki, Takashi, Maki, Koutaro, Kamijo, RyutaroVolume:
12
Language:
english
Journal:
Acta Biomaterialia
DOI:
10.1016/j.actbio.2014.10.038
Date:
January, 2015
File:
PDF, 1.50 MB
english, 2015