Spherical nanoindentation and Vickers microhardness study of the deformation of poled BaTiO[sub 3] single crystals
Buchs, R., Basu, S., Elshrief, O. A., Coward, R., Barsoum, M. W.Volume:
105
Year:
2009
Language:
english
Journal:
Journal of Applied Physics
DOI:
10.1063/1.3117496