Hydrazine and Hydrogen Coinjection to Mitigate Stress Corrosion Cracking of Structural Materials in Boiling Water Reactors (VII)—Effects of Bulk Water Chemistry on ECP Distribution inside a Crack
WADA, Yoichi, ISHIDA, Kazushige, TACHIBANA, Masahiko, AIZAWA, Motohiro, FUSE, MotomasaVolume:
44
Language:
english
Journal:
Journal of Nuclear Science and Technology
DOI:
10.1080/18811248.2007.9711392
Date:
November, 2007