Cerium addition on pitting corrosion of (Cu50Zr50)100–2xCe2x(x=0, 1, 2 and 3) metallic glasses in seawater
ZHANG, Chunzhi, WANG, Jinhuan, QIU, Nannan, XIE, Kun, LI, HuipingVolume:
33
Language:
english
Journal:
Journal of Rare Earths
DOI:
10.1016/S1002-0721(14)60389-6
Date:
January, 2015
File:
PDF, 1.26 MB
english, 2015