Nanotechnology in Construction 3 || Nanoindentation Study of Na-Geopolymers Exposed to High Temperatures
Bittnar, Zdeněk, Bartos, Peter J. M., Němeček, Jiří, Šmilauer, Vít, Zeman, JanVolume:
10.1007/97
Year:
2009
Language:
english
DOI:
10.1007/978-3-642-00980-8_22
File:
PDF, 616 KB