A comparison of high speed differential scanning calorimetry (Hyper-DSC) and modulated differential scanning calorimetry to detect the glass transition of polyvinylpyrrolidone: the effect of water content and detection sensitivity in powder mixtures (a model formulation)
Saklatvala, R.D., Saunders, M.H., Fitzpatrick, S., Buckton, G.Volume:
15
Year:
2005
Language:
english
Journal:
Journal of Drug Delivery Science and Technology
DOI:
10.1016/S1773-2247(05)50046-7