![](/img/cover-not-exists.png)
Nanoindentation of viscoelastic solids: A critical assessment of experimental methods
Herbert, Erik G., Sudharshan Phani, P., Johanns, Kurt E.Language:
english
Journal:
Current Opinion in Solid State and Materials Science
DOI:
10.1016/j.cossms.2014.12.006
Date:
January, 2015
File:
PDF, 653 KB
english, 2015