![](/img/cover-not-exists.png)
Study of GTD-111 Superalloy Microstructural Evolution During High-Temperature Aging and After Rejuvenation Treatments
Turazi, Almir, de Oliveira, Carlos Augusto Silva, Bohórquez, Carlos Enrique Niño, Comeli, Franco WronskiVolume:
4
Language:
english
Journal:
Metallography, Microstructure, and Analysis
DOI:
10.1007/s13632-014-0177-x
Date:
February, 2015
File:
PDF, 8.02 MB
english, 2015