Mechanical Properties and Microstructure of IN738LC Nickel Superalloy Castings
Zýka, Jiří, Andršová, Irena, Podhorná, Božena, Hrbáček, KarelVolume:
782
Language:
english
Journal:
Materials Science Forum
DOI:
10.4028/www.scientific.net/MSF.782.437
Date:
April, 2014
File:
PDF, 1.82 MB
english, 2014