Microstructural examination of V–(Fe or Cr)–Ti alloys after thermal-creep or irradiation-creep tests
K. Fukumoto, S. Takahashi, R.J. Kurtz, D.L. Smith, H. MatsuiVolume:
341
Year:
2005
Language:
english
Pages:
7
DOI:
10.1016/j.jnucmat.2005.01.016