Three dimensional observations and modelling of intergranular stress corrosion cracking in austenitic stainless steel
T.J. Marrow, L. Babout, A.P. Jivkov, P. Wood, D. Engelberg, N. Stevens, P.J. Withers, R.C. NewmanVolume:
352
Year:
2006
Language:
english
Pages:
13
DOI:
10.1016/j.jnucmat.2006.02.042
File:
PDF, 566 KB
english, 2006