![](/img/cover-not-exists.png)
Precipitation in AISI 316L(N) during creep tests at 550 and 600 °C up to 10 years
A.F. Padilha, D.M. Escriba, E. Materna-Morris, M. Rieth, M. KlimenkovVolume:
362
Year:
2007
Language:
english
Pages:
7
DOI:
10.1016/j.jnucmat.2006.12.027
File:
PDF, 1.37 MB
english, 2007