![](/img/cover-not-exists.png)
Effect of Boron Carbide Particle Size and Volume Fraction of TiB-TiC Reinforcement on Fractography of PM Processed Titanium Matrix Composites
Vadayar, K. Srinivasa, Rani, S. Devaki, Prasad, V.V. BhanuVolume:
6
Year:
2014
Language:
english
Journal:
Procedia Materials Science
DOI:
10.1016/j.mspro.2014.07.111
File:
PDF, 2.44 MB
english, 2014