![](/img/cover-not-exists.png)
Mechanical Properties of Titanium–Titanium Boride Composites Through Nanoindentation and Ultrasonic Techniques — An Evaluation Perspective
Selvakumar, M., Chandrasekar, P., Ravisankar, B., Balaraju, J. N., Mohanraj, M.Volume:
53
Language:
english
Journal:
Powder Metallurgy and Metal Ceramics
DOI:
10.1007/s11106-015-9650-6
Date:
January, 2015
File:
PDF, 1.72 MB
english, 2015