Microstructural Characterization of Internal Welding Defects and Their Effect on the Tensile Behavior of FSW Joints of AA2198 Al-Cu-Li Alloy
Le Jolu, Thomas, Morgeneyer, Thilo F., Denquin, Anne, Sennour, Mohamed, Laurent, Anne, Besson, Jacques, Gourgues-Lorenzon, Anne-FrançoiseVolume:
45
Language:
english
Journal:
Metallurgical and Materials Transactions A
DOI:
10.1007/s11661-014-2537-1
Date:
November, 2014
File:
PDF, 3.24 MB
english, 2014