![](/img/cover-not-exists.png)
Differential scanning calorimetry analysis of crystal structure transformation in spray-dried particles consisting of ammonium nitrate, potassium nitrate, and a polymer
Nagayama, Seiichiro, Katoh, Katsumi, Higashi, Eiko, Nakano, Katsuyuki, Kumagae, Kosuke, Habu, Hiroto, Wada, Yuji, Arai, MitsuruVolume:
118
Language:
english
Journal:
Journal of Thermal Analysis and Calorimetry
DOI:
10.1007/s10973-014-4127-2
Date:
November, 2014
File:
PDF, 361 KB
english, 2014