![](/img/cover-not-exists.png)
Fractographical characterization of hot pressed and pressureless sintered SiAlON-doped ZrB2–SiC composites
Shahedi Asl, Mehdi, Nayebi, Behzad, Ahmadi, Zohre, Pirmohammadi, Parinaz, Ghassemi Kakroudi, MahdiVolume:
102
Language:
english
Journal:
Materials Characterization
DOI:
10.1016/j.matchar.2015.03.002
Date:
April, 2015
File:
PDF, 2.13 MB
english, 2015