Impact of binders on viscosity of low-pressure powder injection molded Inconel 718 superalloy
V. Demers,S. Turenne,O. ScalzoVolume:
50
Language:
english
Journal:
Journal of Materials Science
DOI:
10.1007/s10853-015-8853-z
Date:
April, 2015
File:
PDF, 690 KB
english, 2015