![](/img/cover-not-exists.png)
Effective Hf-Pd Co-doped β-NiAl(Cr) coatings for single-crystal superalloys
Adharapurapu, Raghavendra R., Zhu, Jun, Dheeradhada, Voramon S., Lipkin, Don M., Pollock, Tresa M.Volume:
76
Language:
english
Journal:
Acta Materialia
DOI:
10.1016/j.actamat.2014.03.001
Date:
September, 2014
File:
PDF, 3.71 MB